Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 58.0 °C | 136 °F | TM R050-25 |
Resinlab® EP1285HD-16 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Glass Transition Temp, Tg | 58.0 °C | 136 °F | DMA, E" |
Objet FullCure® 830 Vero White Resin for Rapid Prototyping Information provided by American Precision Prototyping, LLC |
|||
Glass Transition Temp, Tg | 58.0 °C | 136 °F | DMA (SYSS) |
RedEye On Demand VeroBlack PolyJet™ FC870 for Rapid Prototyping Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero.. |
|||
Glass Transition Temp, Tg | 58.0 °C | 136 °F | DMA (SYSS) |
RedEye On Demand VeroWhite PolyJet Resin White for Rapid Prototyping Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero.. |
|||
Glass Transition Temp, Tg | 58.0 °C | 136 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® BS3803 Ethylene Vinyl Alcohol Copolymer Modified ET3803; New Stretchable EVOH. Ethylene content 38 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows .. |
|||
Glass Transition Temp, Tg | 58.0 °C | 136 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® ET3803 Ethylene Vinyl Alcohol Copolymer Medium ethylene content. Suitable for packaging a wet product in a wet environment. Preferred for use in forming webs for meat and cheese packaging. Ethylene content 38 mol%. Volatile matter 0.3%... |
|||
Glass Transition Temp, Tg | 58.0 °C | 136 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® ET3808 Ethylene Vinyl Alcohol Copolymer Ethylene content 38 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |
|||
Glass Transition Temp, Tg | 58.0 °C | 136 °F | |
Mallard Creek Polymers Rovene® 4301 Styrene-Butadiene Emulsion Rovene® 4301 is a self crosslinking, carboxylated styrene-butadiene emulsion that has a very stiff hand. The binder is especially recommended for durable nonwovens such as floor maintenance pads .. |
|||
Glass Transition Temp, Tg | 58.0 °C | 136 °F | Ultimate Tg |
Tra-Con Tra-Bond 2137 Easy-Flow No-Sag Epoxy Adhesive TRA-BOND 2137 epoxy adhesive is an easy-to-apply, room temperature cure epoxy adhesive system developed for structural bonding applications on vertical or overhead surfaces where its instant develop.. |
|||
Glass Transition Temp, Tg | 58.0 °C | 136 °F | |
Armstrong A-2/H20 Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |
|||
Glass Transition Temp, Tg | 58.0 °C | 136 °F | DMA, E" |
3D Systems Accura® 60 Plastic for SLA® Systems Simulate the properties and appearance of polycarbonate. For use with solid-state stereolithography (SLA®) systems.ApplicationsTough functional prototypesAutomotive design componentsConsumer electr.. |
|||
Glass Transition Temp, Tg | 58.0 °C | 136 °F | |
3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Glass Transition Temp, Tg | 58.0 °C | 136 °F | DMA, E" |
Proto3000 Objet VeroWhite FullCure830 Rapid Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Glass Transition Temp, Tg | 58.0 °C | 136 °F | DMA, E" |
Proto3000 Accura® 60 Plastic Stereolithography (SLA) Prototyping Polymer Features:Durable and stiffHigh clarityFast build speedLow viscosity formulationHumidity resistant partsFully developed and tested build stylesBenefits:Achieve the look and feel of polycarbonateView .. |