Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 279 °C | 534 °F | Dry, Storage Modulus |
Renegade Materials Corporation RM-3010 Bismaleimide (BMI) Resin for VARTM Developed using state-of-the-art formulating technologies, RM-3010 One-Part BMI VARTM resin delivers superior hot/wet performance in airframe, missile and propulsion applications at service temperat.. |