Material Notes:
Developed using state-of-the-art formulating technologies, RM-3010 One-Part BMI VARTM resin delivers superior hot/wet performance in airframe, missile and propulsion applications at service temperatures up to 400°F. RM-3010 BMI resin delivers improved damage tolerance at higher temperatures vs. industry-standard BMI resins. RM-3010 resin can be injected into a variety of woven and non-crimp fabrics as well as braids and other complex engineered preforms. Its long pot life (< 1000 cps @ 8 hours at 110°C) makes it very suitable for injecting large complex structural parts. Renegade also offers a similar resin system for Resin Transfer Molding (RTM) processing to support molding of smaller, tightly toleranced parts called RM-3000 and an autoclave prepreg version called RM-3002.Information provided by Renegade Materials Corporation.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
Cured; ASTM D790
Mechanical Properties Metric English Comments
Flexural Strength 124 MPa
18000 psi
Flexural Modulus 4.59 GPa
665 ksi
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 252 °C
485 °F
Wet, Storage Modulus (Immersion for 72 hr, 180°F)
279 °C
534 °F
Dry, Storage Modulus
Descriptive Properties Value Comments
Flexural Strain to Failure 2.5%