Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 161 °C | 322 °F | DMA (SYSS) |
RedEye On Demand PC-ISO for Parts that can be Sterilized Polycarbonate-ISO (PC-ISO) is a durable high-performance plastic that meets both ISO 10993-1 and USP Class VI standards in its raw state. PC-ISO can be sterilized using either the gamma radiation or.. |
|||
Glass Transition Temp, Tg | 161 °C | 322 °F | DMA (SYSS) |
RedEye On Demand Polycarbonate High Impact Strength & Temperature Resistant for Rapid Prototyping Polycarbonate (PC) is an actual industrial-grade thermoplastic that is impact-resistant and structurally strong. PC parts are built with a layered manufacturing process utilizing Fused Deposition Mo.. |
|||
Glass Transition Temp, Tg | 161 °C | 322 °F | DSC (SSYS) |
Stratasys® Polycarbonate A true industrial thermoplastic, PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating strong parts .. |
|||
Glass Transition Temp, Tg | 161 °C | 322 °F | DMA (SSYS) |
Stratasys® Polycarbonate-ISO PC-ISO (polycarbonate-ISO), an industrial thermoplastic, in its raw state meets the ISO 10993-1 and USP Class VI classification1 and comes in a variety of colors. Because of their strength and medic.. |
|||
Glass Transition Temp, Tg | 161 °C | 322 °F | DAM (SSYS) |
Proto3000 PC Fused Deposition Modeling Polymer Description: A true industrial thermoplastic, PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating .. |
|||
Glass Transition Temp, Tg | 161 °C | 322 °F | DAM (SSYS) |
Proto3000 PC ISO Fused Deposition Modeling Polymer Description: PC-ISO (polycarbonate-ISO), an industrial thermoplastic, which in its raw state, meets the ISO 10993-1 and USP Class VI classi?cation 1. PC-ISO blends are commonly used in food and drug.. |