Material Notes:
PC-ISO (polycarbonate-ISO), an industrial thermoplastic, in its raw state meets the ISO 10993-1 and USP Class VI classification1 and comes in a variety of colors. Because of their strength and medical compatibility, PCISO blends are commonly used in food and drug packaging and medical device manufacturing. PC-ISO gives you Real Parts™ that can be functionally utilized from conceptual prototyping through design verification through direct digital manufacturing.Information provided by Stratasys®
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 52.0 MPa
7540 psi
Type 1, 2"/min; ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Tensile Modulus 1.744 GPa
252.9 ksi
Type 1, 2"/min; ASTM D638
Flexural Strength 82.0 MPa
11900 psi
ASTM D790
Flexural Modulus 2.193 GPa
318.1 ksi
ASTM D790
Izod Impact, Notched 0.5339 J/cm
1.000 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.805 J/cm
9.002 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 133 °C
271 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
261 °F
ASTM D648
Vicat Softening Point 139 °C
282 °F
ISO 306
Glass Transition Temp, Tg 161 °C
322 °F
DMA (SSYS)
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 2.96

@Frequency 1.00e+6 Hz
2.96

@Frequency 1.00e+6 Hz
IEC 60250
3.17

@Frequency 60.0 Hz
3.17

@Frequency 60.0 Hz
IEC 60250