Thermal Properties Metric English Comments
Glass Transition Temp, Tg 121 °C
250 °F
10°C/min test
Polimeri Europa SINKRAL C350 ABS, Heat Stabilized  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-08-16-25 Heat resistant injection moulding grade. Combines good flow with toughness and high thermal charac..
Glass Transition Temp, Tg 121 °C
250 °F
DSC
Kolon NOPLA® KE931 PEN-PET Copolyester
NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac..
Glass Transition Temp, Tg 121 °C
250 °F
Dry
Hexcel® HexPly® F155 Epoxy Resin
HexPly® F155 is an advanced modified epoxy formulation designed for autoclave curing to offer very high laminate strengths, coupled with increased fracture toughness and adhesive properties. HexPly..
Glass Transition Temp, Tg 121 °C
250 °F
Dry
Hexcel® HexPly® F522 Epoxy Resin
HexPly® F522 is an advanced, modified epoxy formulation designed for autoclave curing to offer very high laminate strengths, coupled with increased fracture toughness, excellent hot-wet properties ..
Glass Transition Temp, Tg 121 °C
250 °F
DSC
DuPont Teijin Films Teonex® Q51 Polyester Film, 48 Gauge
Teonex® Q51 is biaxially oriented polyethylene naphthalate (PEN) film. It is slightly hazy with excellent handling properties for general purpose. It is commercially available in nominal 48 - 1000 ..
Glass Transition Temp, Tg 121 °C
250 °F
DSC
DuPont Teijin Films Teonex® Q83 Polyester Film, 200 Gauge
Teonex® Q83 is biaxially oriented, slightly hazy polyethylene naphthalate (PEN) film with excellent handling properties and high dimensional stability. It is commercially available in 100, 200 and ..
Glass Transition Temp, Tg 121 °C
250 °F
dry
Henkel Hysol EA 9628 Film Adhesive
First generation, modified epoxy film, good stress, environmental resistance and structural propertiesApplications: Composite Bonding, Metal & Honeycomb BondingData from .060 psf, 300 g/m2