Material Notes:
HexPly® F155 is an advanced modified epoxy formulation designed for autoclave curing to offer very high laminate strengths, coupled with increased fracture toughness and adhesive properties. HexPly® F155 is a controlled flow epoxy resin for lamination and co-curing at 250ºF (121ºC) cure. HexPly® F155 will pass MIL-R-9300, co-cure as a honeycomb facing, and bond metal to metal.Information provided by HexCel
Physical Properties Metric English Comments
Specific Gravity 1.335 g/cc
1.335 g/cc
Moisture Absorption at Equilibrium 9.4 %
9.4 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
Elongation at Yield 5.2 %
5.2 %
Tensile Modulus 3.24 GPa
470 ksi
Fracture Toughness 1.65 MPa-m½
1.50 ksi-in½
Thermal Properties Metric English Comments
CTE, linear 52.7 µm/m-°C
29.3 µin/in-°F
Glass Transition Temp, Tg 121 °C
250 °F
Dry
Processing Properties Metric English Comments
Gel Time 4.00 - 10.0 min

@Temperature 121 °C
4.00 - 10.0 min

@Temperature 250 °F