Polymer Property : Glass Transition Temp, Tg = 195 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 195 °C
383 °F
Vyncolit Neopreg Kinel® SK80 L8G Glass Fiber Reinforced Molding Compound
Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited for over mold..
Glass Transition Temp, Tg 195 °C
383 °F
Vyncolit Neopreg Kinel® SK4504 S12 Carbon Reinforced Molding Compound
Epoxy based molding compound long carbon fiber reinforced suited for demanding tribologic applications under dry running conditions, exposed to a wide range of temperatures (-100°C up to 150°C)...