Polymer Property : Glass Transition Temp, Tg = 175 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 175 °C
347 °F
TMA; IPC-TM-650.2.4.24c
Park Electrochemical Nelco® N5000 BT Epoxy Laminate and Prepreg
The Nelco N5000 BT epoxy laminate and prepreg system provides superior electrical properties. The N5000 resin system wasoriginally developed for application specific use in high densitymilitary and ..
Glass Transition Temp, Tg >= 175 °C
>= 347 °F
TMA; IPC-TM-650.2.4.24c
Park Electrochemical Nelco® N4000-29 BC® Buried Capacitance™ Multifunctional Epoxy
The Nelco N4000-29 is a lead-free, low-CTE, high Tg multifunctional epoxy substrate which has been designed for use in standard multilayer PWB designs and today’s toughest, high-performance, lead-f..
Glass Transition Temp, Tg 175 °C
347 °F
Mettler DSC-30, ASTM D3418
Lord Adhesives Thermosetâ„¢ EP-830 Ignition Coil Impregnating and Encapsulation Epoxy
Lord EP-830 is a heat curing, two component epoxy formulation designed especially for use in automotive high voltage ignition coils where adhesion to segmented bobbins is critical. The combination o..
Glass Transition Temp, Tg >= 175 °C
>= 347 °F
Master Bond EP30-3LO Highly versatile, two part epoxy system for bonding, coating, sealing and casting
Master Bond EP30-3LO is a two component epoxy system featuring a combination of optical clarity and light transmission, good glass transition temperature (Tg), great chemical resistance along with p..
Glass Transition Temp, Tg >= 175 °C
>= 347 °F
DSC; IPC-TM-650.2.4.25c
Park Electrochemical Nelco® N4000-11 BC® Buried Capacitance™ Epoxy Laminate and Prepreg
The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved..
Glass Transition Temp, Tg >= 175 °C
>= 347 °F
TMA; IPC-TM-650.2.4.24c
Park Electrochemical Nelco® N4000-29 Multifunctional Epoxy
The Nelco N4000-29 is an advanced, lead-free, low-CTE, high Tg (185º C by DSC) multifunctional epoxy dielectric substrate. This material has been designed for use not only in standard multilayer PW..
Glass Transition Temp, Tg 175 °C
347 °F
DSC; Nominal; IPC-TM-650.2.4.25c
Park Electrochemical Nelco® N4000-6 FC Multifunctional Epoxy Laminate and Prepreg
The Nelco® N4000-6 FC is a high-Tg epoxy laminate and prepreg system that provides a wide range of performance versatility and ease of processing for demanding high-layer count applications.Key Fea..
Glass Transition Temp, Tg 175 °C
347 °F
DSC; IPC TM-650 2.4.25
Arlon 45N Multifunctional Epoxy Laminate and Prepreg
Arlon 45N is a tough, high Tg (175°C by DSC) multifunctional epoxy laminate and prepreg system designed for use in a variety of higher layer count MLBs. Processable using conventional FR-4 conditi..
Glass Transition Temp, Tg >= 175 °C
>= 347 °F
DSC; IPC-TM-650.2.4.25c
Park Electrochemical Nelco® N4000-11 Multifunctional Epoxy Laminate and Prepreg
The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved..
Glass Transition Temp, Tg 175 °C
347 °F
DSC; IPC TM-650 2.4.25
Arlon 44N Multifunctional Microdispersed Ceramic Filled Epoxy-Fiberglass Prepreg
Arlon 44N is a high resin content multifunctional (175°C) epoxy prepreg system with a proprietary microdispersed ceramic filler system. 44N is engineered for the filling of clearance holes in thi..