Park Electrochemical Nelco® N4000-11 BC® Buried Capacitance™ Epoxy Laminate and Prepreg

Category Polymer , Thermoset , Epoxy
Manufacturer Park Electrochemical Corp.
Trade Name Nelco®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Park Electrochemical Nelco® N4000-11 BC® Buried Capacitance™ Epoxy Laminate and Prepreg.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved thermal, mechanical, and electrical performance in lead-free assembly and high layer count, sophisticated PWB designs. The Nelco N4000-11 BC® is offered as a buried capacitance solution, offering a greater degree of design freedom for smaller, more reliable assemblies.Key Features and Benefits:Tg >175ºC, thermal stability and moisture resistanceCAF ResistantLow Z-axis expansionDicyandiamide (DICY) free, proprietary resin chemistrySuperior electrical propertiesBuried Capacitance SolutionOptimized FR-4 processingApplications/Qualifications:High Density InterconnectsLead-Free Assembly SubstrateLarge Format BackplanesTight Tolerance Via to Via ApplicationsHigh I / O Count BGA SubstratesExtreme Layer count MultilayersLead-Free DCA ApplicationsHigh Temperature Underhood AutomotiveTelecommunications InfrastructureSophisticated Data Storage ApplicationsRoHS CompliantMeets IPC-4101/28, /83, /98, /99 SpecificationsInformation provided by Park Electrochemical Corp.
Physical Properties Metric English Comments
Density 1.96 g/cc
0.0708 lb/in³
50% Resin Content; Internal Method
Water Absorption 0.15 %
0.15 %
IPC-TM-650.2.6.2.1
Mechanical Properties Metric English Comments
Peel Strength 1.23 kN/m
7.00 pli
at elevated temperature; IPC-TM-650.2.4.8.2a
1.58 kN/m
9.00 pli
after exposure to process solutions; IPC-TM-650.2.4.8
1.58 kN/m
9.00 pli
after solder float; IPC-TM-650.2.4.8
Thermal Properties Metric English Comments
Specific Heat Capacity 1.21 - 1.38 J/g-°C
0.290 - 0.330 BTU/lb-°F
ASTM E1461-92
Thermal Conductivity 0.401 - 0.599 W/m-K
2.78 - 4.16 BTU-in/hr-ft²-°F
ASTM E1461-92
Glass Transition Temp, Tg 170 °C
338 °F
TMA; IPC-TM-650.2.4.24c
>= 175 °C
>= 347 °F
DSC; IPC-TM-650.2.4.25c
Decomposition Temperature 345 °C
653 °F
5% weight loss; TGA; IPC-TM-650.2.4.24.6
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 3.5

@Frequency 1.00e+9 Hz
3.5

@Frequency 1.00e+9 Hz
RF Impedance; IPC-TM-650.2.5.5.9
3.5

@Frequency 2.50e+9 Hz
3.5

@Frequency 2.50e+9 Hz
Stripline; IPC-TM-650.2.5.5.5
3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
TFC/LCR Meter; IPC-TM-650.2.5.5.3
Dielectric Strength 51.2 kV/mm
1300 kV/in
IPC-TM-650.2.5.6.2
Dissipation Factor 0.015

@Frequency 2.50e+9 Hz
0.015

@Frequency 2.50e+9 Hz
Stripline; IPC-TM-650.2.5.5.5
0.018

@Frequency 1.00e+6 Hz
0.018

@Frequency 1.00e+6 Hz
TFC/LCR Meter; IPC-TM-650.2.5.5.3
Descriptive Properties Value Comments
Methylene Chloride Resistance (% Weight Change) 0.8
IPC-TM-650.2.3.4.3
T260 (minutes) 30
IPC-TM-650.2.4.24.1