Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 74.0 °C | 165 °F | DSC |
ExxonMobil Escor® AT-310 EMAAA Terpolymer for Polymer Modification
(discontinued **) Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components such as aluminum foil, polyolefins, polycarbonate, PET, e.. |
|||
Glass Transition Temp, Tg | 74.0 °C | 165 °F | ASTM E1545-00 |
DSM Somos® ProtoTherm™ 12120 Water-resistant resin for stereolithography, UV Postcure DescriptionDSM Somos® 12120 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12120 have a cherry-red appearance which tur.. |
|||
Glass Transition Temp, Tg | 73.9 °C | 165 °F | |
Gromax Evasin EV-3201V Ethylene-Vinyl Alcohol Copolymer Unmodified random Co-Polymer of [Ethylene-Vinyl alcohol], designed for therm-plastic processing into Sheets and Foils with high Oxygen and Aroma Barrier EffectInformation provided by Gromax Enterpri.. |