Thermal Properties Metric English Comments
Glass Transition Temp, Tg 61.0 °C
142 °F
DSC, both heating and cooling speeds of 20°C/min
Noltex Soarnol® ST110 Ethylene Vinyl Alcohol Copolymer
Modified DC3203; improved flex crack resistance and thermoformability. Ethylene content 32 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of n..
Glass Transition Temp, Tg 61.0 °C
142 °F
TM R050-25
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting ..
Glass Transition Temp, Tg 61.0 °C
142 °F
DSC, both heating and cooling speeds of 20°C/min
Noltex Soarnol® DC3212 Ethylene Vinyl Alcohol Copolymer
Ethylene content 32 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a..
Glass Transition Temp, Tg 61.0 °C
142 °F
Armstrong A-34 Epoxy Adhesive
This white paste material is a fast-curing adhesive with a working life of 20-25 minutes in a 100-gram mass. Mixing ratio is a convenient 1:1. A-34 has excellent wetting properties and is suggeste..
Glass Transition Temp, Tg 61.0 °C
142 °F
TM R050-25
Resinlab® EP965 Black Unfilled Electronic Grade Epoxy Encapsulant