Polymer Property : Glass Transition Temp, Tg = 132 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 55.0 - 132 °C
131 - 270 °F
Average value: 92.8 °C Grade Count:6
Overview of materials for Epoxy, Cast, Metal Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a..