Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -69.0 - -17.0 °C | -92.2 - 1.40 °F | Average value: -40.2 °C Grade Count:49 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Glass Transition Temp, Tg | -69.0 °C | -92.2 °F | |
Lubrizol Estane® 2103-70A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: High MVTRAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |