Thermal Properties Metric English Comments
Glass Transition Temp, Tg -52.2 °C
-62.0 °F
reported value is for pure FLEXOMER™ DFDB-1085 NT, the primary component in this blend; Dow Method
Dow FLEXOMER™ DFDA-1095 NT Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ DFDA-1095 NT is an ethylene-butene copolymer with a unique olefinic composition for improved process-ability and material handling. This product is produced via gas phase polymerization ..
Glass Transition Temp, Tg -52.2 °C
-62.0 °F
Dow Method
Dow FLEXOMER™ DFDB-9042 NT Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ DFDB-9042 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It has value as a sealant layer in multilayer film structures for dry and liquid packaging. I..