Thermal Properties Metric English Comments
Glass Transition Temp, Tg -47.2 °C
-53.0 °F
DSC, 10ºC/min; DIN 51.007
Lubrizol Advanced Materials PEARLTHANE® 16N80 Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 16N80 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties and excellent hydrolys..
Glass Transition Temp, Tg -47.2 - -34.8 °C
-53.0 - -30.6 °F
Zeon Chemicals Nipol® 1094-80 Nitrile Elastomer
Nipol 1094-80 is a copolymer of butadiene and acrylonitrile with low oil resistance, developed for low temperature flexibility. Sufficient non-staining antioxidant is added during manufacture for no..
Glass Transition Temp, Tg -47.2 °C
-53.0 °F
HR 10 K/min; half height; DSC
Dow SE SLR-4400 Solution polymerized Styrene Butadiene Rubber (S-SBR)
SE SLR-4400 is manufactured by anionic solution polymerization using lithium initiator. It is a product with medium styrene and high vinyl content. The product is partially Sn-coupled and non-stai..