Lubrizol Advanced Materials PEARLTHANE® 16N80 Thermoplastic Polyurethane Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLTHANE® 16N80 Thermoplastic Polyurethane Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PEARLTHANE® 16N80 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties and excellent hydrolysis and microbe resistance. It can be extruded and injection-moulded. PEARLTHANE® 16N80 can be used for blown- and cast films, cables, tubing and profiles. When processed by injection moulding, can be used for making technical parts.All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 21.6 kg
10 g/10 min

@Load 47.6 lb
Mechanical Properties Metric English Comments
Hardness, Shore A 81
81
ASTM D2240
Tensile Strength 35.00 MPa
5076 psi
ASTM D412
Elongation at Break 760 %
760 %
ASTM D412
100% Modulus 0.00500 GPa
0.725 ksi
ASTM D412
300% Modulus 0.00800 GPa
1.16 ksi
ASTM D412
Tear Strength 80.6 kN/m
460 pli
ASTM D624 (Die C)
Abrasion 20
20
loss (mm³); DIN 53.516
Compression Set 30 %

@Temperature 22.8 °C,
Time 252000 sec
30 %

@Temperature 73.0 °F,
Time 70.0 hour
ASTM D395
42 %

@Temperature 70.0 °C,
Time 86400 sec
42 %

@Temperature 158 °F,
Time 24.0 hour
ASTM D395
Thermal Properties Metric English Comments
Melting Point 160 - 170 °C
320 - 338 °F
MQSA 111
Glass Transition Temp, Tg -47.2 °C
-53.0 °F
DSC, 10ºC/min; DIN 51.007
Processing Properties Metric English Comments
Feed Temperature 179 °C
355 °F
Nozzle Temperature 193 °C
380 °F
Zone 1 179 - 193 °C
355 - 380 °F
Zone 2 191 - 210 °C
375 - 410 °F
Zone 3 199 - 221 °C
390 - 430 °F
Zone 4 185 - 199 °C
365 - 390 °F
Die Temperature 185 - 193 °C
365 - 380 °F
Mold Temperature 35.0 °C
95.0 °F
Moisture Content <= 0.10 %
<= 0.10 %
MQSA 44
Screw Speed 50 rpm
50 rpm