Polymer Property : Glass Transition Temp, Tg = -36.1 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -36.1 °C
-33.0 °F
DSC, 50ºF / min.; ISO11357-2
Lubrizol Advanced Materials PEARLTHANE® D11H95S Thermoplastic Polyurethane Elastomer
PEARLTHANE® D11H95S is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring excellent flow and mechanical properties and an out..