Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -36.1 °C | -33.0 °F | DSC, 50ºF / min.; ISO11357-2 |
Lubrizol Advanced Materials PEARLTHANE® D11H95S Thermoplastic Polyurethane Elastomer PEARLTHANE® D11H95S is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring excellent flow and mechanical properties and an out.. |