Glass Transition Temp, Tg -33.1 - -25.6 °C
-27.6 - -14.1 °F
Zeon Chemicals HyTemp® PV-04 AR Polyacrylate Elastomer
HyTemp PV-04 contains one or more acrylic esters. This polymer is specific to the peroxide vulcanized cure system.Peroxide curable elastomer suitable for O-rings, seals, and gaskets. Also used for b..