Zeon Chemicals HyTemp® PV-04 AR Polyacrylate Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name HyTemp®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals HyTemp® PV-04 AR Polyacrylate Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HyTemp PV-04 contains one or more acrylic esters. This polymer is specific to the peroxide vulcanized cure system.Peroxide curable elastomer suitable for O-rings, seals, and gaskets. Also used for binders, adhesives, caulks, and plastics modification.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Mooney Viscosity 25 - 40

@Temperature 100 °C
25 - 40

@Temperature 212 °F
(1+4); Zeon Test #404
Ash <= 0.60 %
<= 0.60 %
Zeon Test #873
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Gehman T100
Glass Transition Temp, Tg -33.1 - -25.6 °C
-27.6 - -14.1 °F
Descriptive Properties Value Comments
% Volume Swell 45
Curesite Proprietary
Gel-Mek (%), max 40
Heat Loss (%) Max 0.7