Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -35.0 - -25.0 °C | -31.0 - -13.0 °F | |
Zeon Chemicals Nipol® 1432T Nitrile Powder and Crumb Elastomer Nipol 1432T is a copolymer of butadiene and acrylonitrile of medium-high acrylonitrile content. Sufficient antioxidant is added during manufacture for normal storage conditions.Used in adhesives and.. |
|||
Glass Transition Temp, Tg | -35.0 - -25.0 °C | -31.0 - -13.0 °F | |