Polymer Property : Glass Transition Temp, Tg = -31.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
Multibase Multi-Flex® TPE D 4502 BLK
Multi-Flex® D 4502 is based on Shell's Kraton G polymer and is suitable for applications for the automotive industry. It exhibits excellent paintability adhesion and is recommended as substrate fo..
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
Multibase Multi-Flex® TPO D 4508 D 4508
This product is suitable for airbag enclosures and is based on polyolefins/kraton rubber, exhibiting good paintability and low temperature performance.Data provided by Multibase.
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
Reliance Industries METABOLIX PHO
Information provided by Reliance Industries
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
ASTM D3417
REXtac Rextac® RT 2880 Amorphous Polyalphaolefin (APAO)
Adhesive and Sealant Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Very low softening point and excellent tensile propertiesApplications: Component of hot melt adhesives, sealants..
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
DMTA
Solvay Specialty Polymers Solef® 8808/0902 Carbon Fiber Reinforced PVDF Compound  (discontinued **)
Key features of this grade: Carbon Fiber Reinforcement, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinate..
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
Midpoint; ASTM E 1269
Huntsman IROGRAN® PS 440-200 TPU-Polyester
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
Mallard Creek Polymers ROVENE® 5044 SBR Latex
ROVENE® 5044 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion specifically designed for formulation of permanent label and construction adhesives. Its relative low molecular w..
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
ASTM E1356
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)
Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Features: Copolymer; Good Flexibility; Medium ViscosityAdditional Properties: Crystal..
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
Styron Enversaâ„¢ 705A Formulated SB
Performance Features: ENVERSAâ„¢ Cushion Technology, excellent recovery, cushion, excellent acoustic propertiesApplications: Sound DampeningEuropeInformation provided by Styron
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
Styron XZ 97224.00 Carboxylated SB
Performance Features: Good compatibility with natural latex, flexibilityApplications: Leather BindingEuropeInformation provided by Styron
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
Wanhua Chemical Wanthane® WHT-A895 Aliphatic TPU
Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Glass Transition Temp, Tg -35.0 - -25.0 °C
-31.0 - -13.0 °F
Zeon Chemicals Nipol® 1432T Nitrile Powder and Crumb Elastomer
Nipol 1432T is a copolymer of butadiene and acrylonitrile of medium-high acrylonitrile content. Sufficient antioxidant is added during manufacture for normal storage conditions.Used in adhesives and..
Glass Transition Temp, Tg -35.0 - -25.0 °C
-31.0 - -13.0 °F
Zeon Chemicals Nipol® 1442 Nitrile Powder and Crumb Elastomer
Nipol 1442 is a copolymer of butadiene and acrylonitrile with medium-high acrylonitrile content. Nipol 1442 shall be in the form of nominal 1/4" three-dimensional chips containing approximately 5%mi..
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
DSC
Lubrizol Estane® AG 9550 Thermoplastic Polyurethane
Type: Estane® AG 9550 is a polyether based aliphatic polyurethane designed for flat die extrusion into film and sheet products.Features: Very tough, high modulus, high tear and tensile properties t..
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
10°C/min
Covestro Texin® 4210 Urethane Thermoplastic Elastomer
Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience w..
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
10°C/min
Covestro Texin® 4215 Urethane Thermoplastic Elastomer
Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience w..
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
DSC, 10°C/min (inf); DuPont Test
Dow Engage® ENR 7086.01 Ethylene-Butene Copolymer
Description: ENR 7086.01 is a revolutionary new ethylene-butene copolymer with a broader molecular weight distribution and much higher levels of long chain branching than other commercially availabl..
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
Cured property; ASTM E831-86
Aptek UVISTAKE 7205LM-PMF UV Curing, Low Outgassing, Urethane staking compound
UVISTAKE 7205LM-PMF is a 100% solids, thixotropic, one component, premixed frozen, electrically insulating, urethane system designed for the attachment and staking of electrical/electronic component..
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
ASTM D4065
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
Pellet sample
BASF Elastollan® 1190A10 Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.