Polymer Property : Specific Heat Capacity = 2.80 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.20 - 2.80 J/g-°C
0.287 - 0.669 BTU/lb-°F
Rotuba 855, Slow Burning Ethyl Cellulose
Data provided by the manufacturer.
Specific Heat Capacity 1.20 - 2.80 J/g-°C
0.287 - 0.669 BTU/lb-°F
Rotuba 856, Slow Burning Ethyl Cellulose
Data provided by the manufacturer.