Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.20 - 2.80 J/g-°C | 0.287 - 0.669 BTU/lb-°F | |
Rotuba 855, Slow Burning Ethyl Cellulose Data provided by the manufacturer. |
|||
Specific Heat Capacity | 1.20 - 2.80 J/g-°C | 0.287 - 0.669 BTU/lb-°F | |
Rotuba 856, Slow Burning Ethyl Cellulose Data provided by the manufacturer. |