Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.77 J/g-°C | 0.662 BTU/lb-°F | Melt value |
BASF Capron® 8362 HS Impact Modified, 34% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8362 HS is a 34% glass reinforced, impact modified, heat stabilized nylon6 injection molding compound exhibiting a high level of toughness in combination with excellent processability and sur.. |