Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.13 J/g-°C | 0.509 BTU/lb-°F | Average value: 2.13 J/g-°C Grade Count:3 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Specific Heat Capacity | 2.13 J/g-°C | 0.509 BTU/lb-°F | |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) 33% Glass Reinforced Polyamide 612 Developed for Electrical and Electronics Applications Zytel FE5382 BK276 is a 33% glass fiber reinforced heat stabilized black polyamide 612 resin developed for el.. |
|||
Specific Heat Capacity | 2.13 J/g-°C | 0.509 BTU/lb-°F | |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612 33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Specific Heat Capacity | 2.13 J/g-°C | 0.509 BTU/lb-°F | |
Styron Magnum™ 9020 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |