Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.12 J/g-°C | 0.507 BTU/lb-°F | |
Styron Magnum™ 344HP ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |