Polymer Property : Specific Heat Capacity = 0.507 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 2.12 J/g-°C
0.507 BTU/lb-°F
Styron Magnumâ„¢ 344HP ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..