Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.21 - 2.04 J/g-°C | 0.290 - 0.488 BTU/lb-°F | Average value: 1.61 J/g-°C Grade Count:7 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |