Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.21 J/g-°C | 0.290 BTU/lb-°F | |
Owens Corning Glass Fiber Reinforced Polycarbonate, 10 wt.% glass Data provided by the manufacturer, Owens Corning. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.290 BTU/lb-°F | ASTM E1461 |
Park Electrochemical Nelco® N4000-7 SI® FR-4 Epoxy Laminate and Prepreg The Nelco® N4000-7 low-CTE epoxy laminate and prepreg system is a cost-effective solution for use in a broad range of multilayer PCB designs requiring low Z-axis expansion, excellent thermal stabil.. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 500 PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 500 PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 500R PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 500R PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 503 PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 503 PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 503R PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 503R PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.290 BTU/lb-°F | ASTM E1461 |
Park Electrochemical Nelco® N4000-13 BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. The Nelco N4000-13 BC® is offered as a.. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.290 BTU/lb-°F | ASTM E1461 |
Park Electrochemical Nelco® N4000-13 EP™ BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg Nelco N4000-13 EP™ is an enhanced epoxy resin system engineered for today’s leadfree requirements where multiple solder reflow at temperatures approaching 260ºC are required. N4000-13 EP provides.. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.290 BTU/lb-°F | ASTM E1461 |
Park Electrochemical Nelco® N4000-13 High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic.. |
|||
Specific Heat Capacity | 1.21 - 1.38 J/g-°C | 0.290 - 0.330 BTU/lb-°F | ASTM E1461-92 |
Park Electrochemical Nelco® N4000-2 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-2 is the most established material of Nelco’s product line. This multifunctional epoxy laminate and prepreg system has a long history of use and one of the broadest operating and .. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.290 BTU/lb-°F | ASTM E1461 |
Park Electrochemical Nelco® N4000-7 FR-4 Epoxy Laminate and Prepreg The Nelco® N4000-7 low-CTE epoxy laminate and prepreg system is a cost-effective solution for use in a broad range of multilayer PCB designs requiring low Z-axis expansion, excellent thermal stabil.. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.290 BTU/lb-°F | ASTM E1461 |
Park Electrochemical Nelco® N4350-13 RF Microwave Performance, Modified Epoxy The Nelco N4350-13 RF and N4380-13 RF series are enhanced epoxy resin systems specifically engineered to provide a unique solution for design applications that demand outstanding thermal properties,.. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.290 BTU/lb-°F | ASTM E1461 |
Park Electrochemical Nelco® N4380-13 RF Microwave Performance, Modified Epoxy The Nelco N4350-13 RF and N4380-13 RF series are enhanced epoxy resin systems specifically engineered to provide a unique solution for design applications that demand outstanding thermal properties,.. |
|||
Specific Heat Capacity | 1.21 - 1.81 J/g-°C | 0.289 - 0.433 BTU/lb-°F | Average value: 1.40 J/g-°C Grade Count:6 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Specific Heat Capacity | 1.21 - 2.04 J/g-°C | 0.290 - 0.488 BTU/lb-°F | Average value: 1.61 J/g-°C Grade Count:7 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | R&H P-37 |
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines.. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | |
Hippe PBT Polybutylene Terephthalate The mechanical properties of PBT are generally inferior to the partially crystallized PET, however, PBT is more easily machined.Information provided by Hippe. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | |
Azoty Tarnow™ TARNOFORM 300 GF4 POM 20% glass fiber reinforced injection molding grade with very high strength.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | |
Azoty Tarnow™ TARNOFORM 300 GF6 POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | |
Azoty Tarnow™ TARNOFORM 300 GF7 POM 35% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | |
Azoty Tarnow™ TARNOFORM 500 GF6 POM 30% glass fiber reinforced, high flow injection molding grade, suitable for applications where high strength and stiffness is required, combined with higher flowability during molding.Information pr.. |
|||
Specific Heat Capacity | 1.21 - 1.38 J/g-°C | 0.290 - 0.330 BTU/lb-°F | ASTM E1461-92 |
Park Electrochemical Nelco® N4000-11 BC® Buried Capacitance™ Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | |
3M Novec™ 7200 Engineered Fluid 3M™ Novec™ 7200 fluid's convenient boiling point and excellent environmental, health and safety profile make it useful as a heat transfer fluid, cleaning solvent, for lubricant deposition & many m.. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | |
3M Novec™ 7200DL Engineered Fluid A high-purity version of 3M™ Novec™ 7200, 3M™ Novec™ 7200DL is tightly-controlled for ions, metals and non-volatile residue. It is used when an application calls for high-purity materials, or a .. |
|||
Specific Heat Capacity | 1.21 - 1.38 J/g-°C | 0.290 - 0.330 BTU/lb-°F | ASTM E1461-92 |
Park Electrochemical Nelco® N4000-6 FC Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-6 FC is a high-Tg epoxy laminate and prepreg system that provides a wide range of performance versatility and ease of processing for demanding high-layer count applications.Key Fea.. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.290 BTU/lb-°F | ASTM E1461 |
Park Electrochemical Nelco® N4000-12 High Speed/Low Loss, CAF Resistant Laminate and Prepreg The Nelco® N4000-12 series is an enhanced epoxy resin system designed for use in high speed, low loss applications requiring thermal stability, excellent signal speed and CAF resistance.Key Feature.. |