Thermal Properties Metric English Comments
Specific Heat Capacity 1.76 J/g-°C
0.421 BTU/lb-°F
Melt
Covestro Bayblend® KU 2-1446 Polycarbonate + ABS Blend  (discontinued **)
Key Features:UnfilledPlatableSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bay..
Specific Heat Capacity 1.76 J/g-°C
0.421 BTU/lb-°F
Styron CALIBREâ„¢ IM 401 11 Polycarbonate, Impact Modified
CALIBRE® IM401 series resins are impact modified, UL listed polycarbonate resins which contain mold release. CALIBRE IM401 polycarbonate resins exhibit an excellent balance of impact strength and..
Specific Heat Capacity 1.76 J/g-°C
0.420 BTU/lb-°F
ExxonMobil Exxon Hyjet V
Exxon HyJet V is a Type V fire-resistant phosphate ester hydraulic fluid, which is superior in thermal and hydrolytic stability to commercially available Type IV hydraulic fluids. Better stability m..
Specific Heat Capacity 1.76 J/g-°C
0.421 BTU/lb-°F
Melt
Covestro Bayblend® T45 PG Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 112 °Cfor electroplating applicationsPreprocessingMax. Water content
Specific Heat Capacity 1.76 J/g-°C
0.421 BTU/lb-°F
Melt
Covestro Bayblend® T45 Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 112 °CPreprocessingMax. Water content
Specific Heat Capacity 1.76 J/g-°C
0.421 BTU/lb-°F
Melt
Covestro Bayblend® T50 XF Polycarbonate + ABS
Injection molding gradeVicat/B 120 = 115 °Cexcellent flowgood low temperature impact strengthPreprocessingMax. Water content
Specific Heat Capacity 1.76 J/g-°C
0.421 BTU/lb-°F
Melt
Covestro Bayblend® T65 XF Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 120 °Cimproved flowability compared to T65PreprocessingMax. Water content
Specific Heat Capacity 1.76 J/g-°C
0.421 BTU/lb-°F
Melt
Covestro Makroblend® DP 7645 Polycarbonate + PET, Impact Grade
Developmental productISO 7792-PC/PET,MHPR,-020(PC/PET)-blends, impact modifiedInjection molding gradeunreinforcedPreprocessingMax. Water content
Specific Heat Capacity 1.76 J/g-°C
0.421 BTU/lb-°F
DuPont 990 test
DuPont™ Tedlar® TUT10BG3 UV Screening Transparent Polyvinyl Fluoride Film
Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o..
Specific Heat Capacity 1.76 J/g-°C
0.420 BTU/lb-°F
ExxonMobil Exxon Hyjet V
Exxon HyJet V is a Type V fire-resistant phosphate ester hydraulic fluid, which is superior in thermal and hydrolytic stability to commercially available Type IV hydraulic fluids. Better stability m..
Specific Heat Capacity 1.76 J/g-°C
0.421 BTU/lb-°F
Melt
Covestro Bayblend® KU 1-1446* Polycarbonate + ABS