Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.920 J/g-°C | 0.220 BTU/lb-°F | ASTM E1461-92 |
Park Electrochemical Nelco® N4000-29 BC® Buried Capacitance™ Multifunctional Epoxy The Nelco N4000-29 is a lead-free, low-CTE, high Tg multifunctional epoxy substrate which has been designed for use in standard multilayer PWB designs and today’s toughest, high-performance, lead-f.. |
|||
Specific Heat Capacity | 0.920 J/g-°C | 0.220 BTU/lb-°F | |
Mateck Magnesium Fluoride (MgF2) Optical crystals |
|||
Specific Heat Capacity | 0.920 J/g-°C | 0.220 BTU/lb-°F | ASTM E1269 |
CoorsTek AD-85 Alumina (nom. 85% Al2O3) Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Specific Heat Capacity | 0.920 J/g-°C | 0.220 BTU/lb-°F | ASTM E1269 |
CoorsTek AD-90 Alumina (nom. 90% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Specific Heat Capacity | 0.920 J/g-°C @Temperature 100 °C |
0.220 BTU/lb-°F @Temperature 212 °F |
Silicone Property; ASTM E1952 |
Arlon Thermabond® R37260N008 0.008" Uncured Silicone Rubber on Fiberglass Carrier Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 m.. |
|||
Specific Heat Capacity | 0.920 J/g-°C | 0.220 BTU/lb-°F | ASTM E1461-92 |
Park Electrochemical Nelco® N4000-29 Multifunctional Epoxy The Nelco N4000-29 is an advanced, lead-free, low-CTE, high Tg (185º C by DSC) multifunctional epoxy dielectric substrate. This material has been designed for use not only in standard multilayer PW.. |