Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.795 J/g-°C | 0.190 BTU/lb-°F | |
Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Specific Heat Capacity | 0.795 J/g-°C @Temperature 20.0 - 800 °C |
0.190 BTU/lb-°F @Temperature 68.0 - 1470 °F |
|
Zircar Ceramics MICROSIL Microporous Insulation MICROSIL Microporous Insulation is an insulation material. Having thermal conductivity an order of magnitude lower than ceramic fiber materials Microsil Microporous Insulation can be an integral par.. |