Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zircar Ceramics MICROSIL Microporous Insulation

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Zircar Ceramics
Trade Name MICROSIL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zircar Ceramics MICROSIL Microporous Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MICROSIL Microporous Insulation is an insulation material. Having thermal conductivity an order of magnitude lower than ceramic fiber materials Microsil Microporous Insulation can be an integral part of thousands of thermal management applications with temperatures as high as 950C (1742F). MICROSIL is a combination of ultra-fine silica powders, specially processed refractory oxides and glass reinforcing fibers. Compacted under tons of force to form a light weight yet rigid structure MICROSIL offers maximum insulation in a minimum amount of space, saving weight and energy. Unique to MICROSIL's microporous structure is its low density which minimizes conductive heat transfer and its billions of nano-pockets which block convection and reflect heat energy – like mirrors – back to its source. MICROSIL is nearly immune to thermal shock. It is completely non-combustible in accordance with standard DIN 4102 Class A1 and can be stored indefinitely in dry conditions. MICROSIL's microporous structure is adversely effected by water, oil, alcohol and other liquids.Information provided by Zircar.
Physical Properties Metric English Comments
Density 0.230 g/cc
0.00831 lb/in³
Mechanical Properties Metric English Comments
Compressive Strength 1.10 MPa
160 psi
Cold Crushing Strength
Compression Set 2.9 %
2.9 %
Compression at 14 psi
Thermal Properties Metric English Comments
Specific Heat Capacity 0.795 J/g-°C

@Temperature 20.0 - 800 °C
0.190 BTU/lb-°F

@Temperature 68.0 - 1470 °F
Thermal Conductivity 0.0190 W/m-K

@Temperature 20.0 °C
0.132 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
0.0230 W/m-K

@Temperature 200 °C
0.160 BTU-in/hr-ft²-°F

@Temperature 392 °F
0.0280 W/m-K

@Temperature 400 °C
0.194 BTU-in/hr-ft²-°F

@Temperature 752 °F
0.0300 W/m-K

@Temperature 600 °C
0.208 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.0380 W/m-K

@Temperature 800 °C
0.264 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Maximum Service Temperature, Air 950 °C
1740 °F
Shrinkage 1.00 %

@Temperature 800 °C,
Time 86400 sec
1.00 %

@Temperature 1470 °F,
Time 24.0 hour
4.80 %

@Temperature 1000 °C,
Time 86400 sec
4.80 %

@Temperature 1830 °F,
Time 24.0 hour
Optical Properties Metric English Comments
Emissivity (0-1) 0.95
0.95
Component Elements Properties Metric English Comments
Other 5.0 %
5.0 %
Oxides
SiC 15 %
15 %
SiO2 80 %
80 %
Descriptive Properties Value Comments
Color Grey
Users viewing this material also viewed the following: