Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.741 J/g-°C | 0.177 BTU/lb-°F | |
Mateck Quartz Crystalline (SiO2) Optical crystals |
|||
Specific Heat Capacity | 0.741 J/g-°C | 0.177 BTU/lb-°F | |
Ceramic Process Systems AlSiC-8, 70 vol% SiC Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone.. |
|||
Specific Heat Capacity | 0.741 J/g-°C | 0.177 BTU/lb-°F | |
Ceramic Process Systems AlSiC-9, 63 vol% SiC Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone.. |