Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.544 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.544 J/g-°C
0.130 BTU/lb-°F
Special Metals NIMONIC® Alloy PE16
A precipitation-hardenable nickel-iron-chromium alloy with an addition of molybdenum for solid-solution strengthening. It has good strength and oxidation resistance at temperatures to about 1380°..
Specific Heat Capacity 0.544 J/g-°C

@Temperature 20.0 °C
0.130 BTU/lb-°F

@Temperature 68.0 °F
California Fine Wire Nickel Alloy 99
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Specific Heat Capacity 0.544 J/g-°C

@Temperature 20.0 °C
0.130 BTU/lb-°F

@Temperature 68.0 °F
California Fine Wire Nickel Alloy 99 Nickel Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.