Thermal Properties Metric English Comments
Specific Heat Capacity 0.5397 J/g-°C

@Temperature 0.000 - 100 °C
0.1290 BTU/lb-°F

@Temperature 32.0 - 212 °F
Indium Corp. In2(SO4)3 Indium Sulfate Anhydrous
Indium Sulfate is a grayish-white powder. It is hydroscopic and possesses a monoclinic prism structure. It is available as an anhydrous powder, a hydrated salt with 9 moles of associated water, an..