Material Notes:
Indium Sulfate is a grayish-white powder. It is hydroscopic and possesses a monoclinic prism structure. It is available as an anhydrous powder, a hydrated salt with 9 moles of associated water, and a solution in varying concentrations up to its solubility limit in water. Indium Sulfate is used as a synthesis chemical and as a hardening agent in gold electroplating baths.PropertiesChemical Formula: In2(SO4)3General Description: Grayish white hydroscopic powder; monoclinic prismsPurity Grades Available: 4N (99.99%), 5N (99.999%)UsesChemical synthesisHardening agent in gold electroplating bathsInformation provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 3.438 g/cc
3.438 g/cc
Solubility in Water 53.92 %

@Temperature 20.0 °C
53.92 %

@Temperature 68.0 °F
Molecular Weight 517.81 g/mol
517.81 g/mol
Vapor Pressure 0.0133 bar

@Temperature 645 °C
10.0 torr

@Temperature 1190 °F
Dissociation Pressure
1.20 bar

@Temperature 820 °C
900 torr

@Temperature 1510 °F
Dissociation Pressure
Thermal Properties Metric English Comments
Specific Heat Capacity 0.5397 J/g-°C

@Temperature 0.000 - 100 °C
0.1290 BTU/lb-°F

@Temperature 32.0 - 212 °F
Component Elements Properties Metric English Comments
Indium, In 40.4 - 44.8 %
40.4 - 44.8 %
44.35 %
44.35 %
Theoretical