Polymer Property : Specific Heat Capacity = 0.490 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 2.05 J/g-°C
0.490 BTU/lb-°F
DuPont Performance Polymers Crastin® 6131 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Low Viscosity Polybutylene Terephthalate Crastin 6131 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by..
Specific Heat Capacity 2.05 J/g-°C
0.490 BTU/lb-°F
DuPont Performance Polymers Crastin® FG6130 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)<
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6130 NC010 is an unreinforced medium high viscosity polyb..