Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.03 J/g-°C | 0.485 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0553/23 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Specific Heat Capacity | 2.03 J/g-°C | 0.485 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Polidan® PNT 0555/06 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0555/06 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes... |
|||
Specific Heat Capacity | 2.03 J/g-°C | 0.485 BTU/lb-°F | |
Styron Magnum™ 541 ABS, High Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Specific Heat Capacity | 2.03 J/g-°C | 0.485 BTU/lb-°F | |
Styron Magnum™ 545 ABS, General Purpose MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Specific Heat Capacity | 2.03 J/g-°C | 0.485 BTU/lb-°F | |
Styron Magnum™ 9010 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Specific Heat Capacity | 2.03 J/g-°C | 0.485 BTU/lb-°F | |
Styron Magnum™ 941 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |