Specific Heat Capacity 1.50 - 1.85 J/g-°C
0.359 - 0.442 BTU/lb-°F
Average value: 1.65 J/g-°C Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..