Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.34 - 1.76 J/g-°C | 0.320 - 0.421 BTU/lb-°F | Average value: 1.54 J/g-°C Grade Count:3 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |