Thermal Properties Metric English Comments
Specific Heat Capacity 1.34 J/g-°C
0.320 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics FL405 PC
Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120
Specific Heat Capacity 1.34 J/g-°C
0.320 BTU/lb-°F
Eastman Eastalloy DA105 PC+PET Copolyester/Polycarbonate  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
Specific Heat Capacity 1.34 J/g-°C
0.320 BTU/lb-°F
Average value: 1.34 J/g-°C Grade Count:3
Overview of materials for PCTG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Specific Heat Capacity 1.34 J/g-°C
0.320 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® FL405 PC
Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120
Specific Heat Capacity 1.34 - 1.76 J/g-°C
0.320 - 0.421 BTU/lb-°F
Average value: 1.54 J/g-°C Grade Count:3
Overview of materials for Polycarbonate/PET Polyester Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values..
Specific Heat Capacity 1.34 J/g-°C
0.320 BTU/lb-°F
ASTM D3418
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Specific Heat Capacity 1.34 J/g-°C
0.320 BTU/lb-°F
ASTM C351
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF)
Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Features: High Viscosity; HomopolymerAdditional Properties: Crystallization Heat - ASTM D3418 46.0 ..
Specific Heat Capacity 1.34 J/g-°C
0.320 BTU/lb-°F
Eastman Eastar DN001 PCTG Copolyester
ISO data as provided by the manufacturer, Eastman Chemical
Specific Heat Capacity 1.34 J/g-°C
0.320 BTU/lb-°F
Eastman Eastar DN003 PCTG Copolyester
ISO data as provided by the manufacturer, Eastman Chemical
Specific Heat Capacity 1.34 J/g-°C
0.320 BTU/lb-°F
Eastman Eastar DN004 PCTG Copolyester
ISO data as provided by the manufacturer, Eastman Chemical
Specific Heat Capacity 1.34 J/g-°C
0.320 BTU/lb-°F
Astro Met AmZirOx 86 Zirconia - Zirconium Oxide
General Description:AmZirOx 86 zirconia (Astro Met Zirconium Oxide) is a yttria stabilized zirconia ceramic material which features high strength and toughness making it a candidate material for use..
Specific Heat Capacity 1.34 J/g-°C

@Temperature 25.0 °C
0.320 BTU/lb-°F

@Temperature 77.0 °F
Liquid
Asahi Glass ASAHIKLIN AK-225T Hydrochlorofluorocarbon Solvent
AK-225T is a mixture of AK-225, ethanol, hydrocarbon and stabilizers. This blend was developed for those customers needing a more aggressive defluxer than AK_225AES. It has proven to be effective in..