Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.399 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 105E3V36327 Acetate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 285E0V16304 Cellulose Acetate Butyrate, Clear, Trsp
Applications:DisplaysProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 285E3720005 Butyrate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 307A4000015 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 307A4000018 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 307E0V16310 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 307E4000018 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 350A0096914 Propionate Natural
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 350A4861313 Cellulose Acetate Propionate, Clear, Trsp
Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 360A4861307 Cellulose Acetate Propionate, Clear, Trsp
Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAEase of processingGamma and..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 360A4861316 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 360E0096914 Cellulose Acetate Propionate, Natural, Trsp
Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 360E3V45508 Propionate Water Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 360E3V45512 Propionate Water Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 360E3V45516 Propionate Water Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 360E461312 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 360E4861314 Cellulose Acetate Propionate, Clear, Trsp
Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 371A4000012 Cellulose Acetate Propionate, Clear, Trsp
Applications:OphthalmicsOral HygienePen/stationary suppliesToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, st..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 380A3V32818 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 380A4000015 Cellulose Acetate Propionate, Clear, Trsp
Applications:OphthalmicsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 383A2R30010 Cellulose Acetate Propionate, Natural, Trsp
Applications:Oral HygienePlastics for hygiene feminine productsRecreationalToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 383A4000011 Cellulose Acetate Propionate, Clear, Trsp
Applications:AppliancesFloor carePersonal care and cosmeticsProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, stren..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp
Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 485E3720023 Butyrate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp
Applications:AppliancesConsumer-Personal careProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gl..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
Average value: 1.46 J/g-°C Grade Count:45
Overview of materials for Cellulose Acetate Propionate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
Average value: 1.47 J/g-°C Grade Count:5
Overview of materials for Cellulose Acetate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
Average value: 1.47 J/g-°C Grade Count:33
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value..
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Eastman Tenite 360A4861301 Propionate Clear, Trsp  (discontinued **)
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Specific Heat Capacity 1.65 - 1.67 J/g-°C
0.394 - 0.399 BTU/lb-°F
Average value: 1.65 J/g-°C Grade Count:40
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..
Copyright © lookpolymers.com All Rights Reserved