Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 30 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 123R PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 203 PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 203R PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 223R PC 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 4701R PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. |
|||
Specific Heat Capacity | 1.26 J/g-°C @Temperature 4.00 °C |
0.301 BTU/lb-°F @Temperature 39.2 °F |
ASTM E1269 |
SABIC Innovative Plastics Lexan® FR66 Polycarbonate Film, Flame Retardant Lexan FR66 flame-retardant film is a clear, thin-gauge polycarbonate film with a suede finish on one side and a matte finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® LUX2614 PC (Asia Pacific) 7.0 MFR. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® LUX2614G PC (Europe-Africa-Middle East) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 243R PC (Asia Pacific) 10.5 MFR. UV-stabilized. Improved flame retardance. Internal mold release. |
|||
Specific Heat Capacity | 1.26 J/g-°C @Temperature 4.00 °C |
0.301 BTU/lb-°F @Temperature 39.2 °F |
ASTM E1269 |
SABIC Innovative Plastics Lexan® FR63 Polycarbonate Film, Flame Retardant Lexan FR63 flame-retardant film is a clear, thin-gauge polycarbonate film with a matte finish on one side and a polish finish on the other and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM E1269 |
SABIC Innovative Plastics Lexan® FR735A Polycarbonate Film, Flame Retardant Lexan FR735A is a black, one side velvet, one polish flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good dimensio.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM E1269 |
SABIC Innovative Plastics Valox® FR1 Polybutylene Terephthalate Film, Flame Retardant Valox FR-1 film is a flame retardant thermoplastic polybutylene, terephthalite film offering UL94 VTM-0 performance down to 125 microns and good temperature performance. Valox FR-1 film’s outst.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® 9040 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® 9070 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® R10460 Medium Flame Retardant Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® R10470 Firm General-Purpose Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® R10480 Medium Low Compression Set Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® 9030 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 307A4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 350A4861313 Cellulose Acetate Propionate, Clear, Trsp Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 360E461312 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 360E4861314 Cellulose Acetate Propionate, Clear, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 380A3V32818 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 485E3720023 Butyrate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | |
ERG Aerospace Reticulated Vitreous Carbon (RVC) Glass-like Carbon Foam |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 360A4861301 Propionate Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HPH4504H PPC High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |