Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.377 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.377 J/g-°C
0.0900 BTU/lb-°F
Carlson 70 30 Cu Ni Copper-Nickel Alloy
General DescriptionCarlson alloy 70 30 Cu Ni is a copper nickel alloy with excellent resistance to corrosion and erosion. It is strong and ductile. 70 30 Cu Ni is utilized in areas where high temp..
Specific Heat Capacity 0.377 J/g-°C

@Temperature 20.0 °C
0.0900 BTU/lb-°F

@Temperature 68.0 °F
Carlson 90 10 Cu Ni Copper-Nickel Alloy
General DescriptionCarlson Alloy 90 10 Cu Ni is a copper-based alloy developed as a cost-effective substitute for 70 30 Cu Ni. An addition of approximately 1.4% iron was made to increase its resist..
Copyright © lookpolymers.com All Rights Reserved