Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.377 J/g-°C | 0.0900 BTU/lb-°F | |
Carlson 70 30 Cu Ni Copper-Nickel Alloy General DescriptionCarlson alloy 70 30 Cu Ni is a copper nickel alloy with excellent resistance to corrosion and erosion. It is strong and ductile. 70 30 Cu Ni is utilized in areas where high temp.. |
|||
Specific Heat Capacity | 0.377 J/g-°C @Temperature 20.0 °C |
0.0900 BTU/lb-°F @Temperature 68.0 °F |
|
Carlson 90 10 Cu Ni Copper-Nickel Alloy General DescriptionCarlson Alloy 90 10 Cu Ni is a copper-based alloy developed as a cost-effective substitute for 70 30 Cu Ni. An addition of approximately 1.4% iron was made to increase its resist.. |