Polymer Property : Specific Heat Capacity = 0.340000 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.00 - 1.42256 J/g-°C

@Temperature 100 - 300 °C
0.239 - 0.340000 BTU/lb-°F

@Temperature 212 - 572 °F
Average value: 1.21 J/g-°C Grade Count:2
Overview of materials for Thermoplastic Polyimide, Unfilled