Thermal Properties Metric English Comments
Specific Heat Capacity 0.320 - 1.14 J/g-°C
0.0765 - 0.272 BTU/lb-°F
Average value: 0.864 J/g-°C Grade Count:15
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Specific Heat Capacity 0.320 - 1.26 J/g-°C
0.0765 - 0.301 BTU/lb-°F
Average value: 0.789 J/g-°C Grade Count:20
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..
Specific Heat Capacity 0.320 J/g-°C
0.0765 BTU/lb-°F
Indium Corp. Germanium Corporation® Germanium Metal
Germanium is a hard, brittle, grayish white element. It is transparent to infrared light, which makes it useful for optical materials. It is widely used as a semiconductor and an alloying agent. ..
Specific Heat Capacity 0.320 J/g-°C
0.0765 BTU/lb-°F
Hippe PEEK Polyetheretherketone
PEEK is a crystalline, easily machinable thermoplastic which is characterized by high tensile and constant good electrical properties between 0°-220°C, as well as due to favorable tribological beh..
Specific Heat Capacity 0.320 - 0.370 J/g-°C
0.0765 - 0.0884 BTU/lb-°F
ETREMA Products Terfenol-D Magnetostrictive Smart Material (Tb0.3Dy0.7Fe1.92)
Terfenol-D is the commercial name for Tb0.3Dy0.7Fe1.92; a composition of material that exhibits giant magnetostriction.Magnetostriction is the phenomenon in which an applied magnetic field causes an..
Specific Heat Capacity 0.320 J/g-°C

@Temperature 1227 °C
0.0765 BTU/lb-°F

@Temperature 2241 °F
ATI Wah Chang Niobium
Niobium is a soft, ductile metal which can be cold worked over 90 percent before annealing becomes necessary. In appearance, the metal is somewhat similar to stainless steel. The density of 8.57 gm/..
Specific Heat Capacity 0.320 J/g-°C
0.0765 BTU/lb-°F
ASTM E 1461-01
Arlon R36133N062 0.062" (1.57 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Layer 1: Cured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production ma..